Activated Alumina
Activated Aluminas, Activated Alumina Ball
Activated alumina has many capillary channels with large surface area and can be used as adsorbent, desiccant and catalyst. At the same time, according to the polarity of the adsorbent to determine, water, oxide, acetic acid, alkali and other strong affinity, is a depth of moisture desiccant, is also the adsorption of polar molecules adsorbent.
Product Description
Activated Alumina, there are many micro-paths, so the specific surface is large. It can be used as absorbent, desiccant and catalyst carrier. It is also a kind of trace water desiccant and the pole molecular absorbent, according to the absorbed molecule polarization, the attachment force is strong for water, oxide, acetic acid, alkali ect. Activated alumina defluorinate just as the anion exchange resin, but the selectivity is much strong. The defluorinate effect of the activated alumina is good. The capacity is stable. It has high strength, low abrasion, no soften in water, no expansion, no powdery no crack. It can widely used in the deep drying of cracked gas, ethylene and propylene, hydrogen-generation, air separation, instrument air drying and fluorine treatment for H2O2, also in the absorbing pollution material, such as H2S, SO2, HF and paraffin in the waste gas, especially in the drinking water defluorinate.
Technical Data
Model |
Activated Alumina |
|||||
Appearance |
White, Sphere, No Odor, Insoluble In Water, Innocuous |
|||||
Type |
KA401 |
KA402 |
KA403 |
KA404 |
KA405 |
|
Crystal Type |
x-p |
x-p |
y |
y |
x-p |
|
Chemical Composition |
Al2O3 % |
≥93 |
≥93 |
≥93 |
≥93 |
≥93 |
Na2O % |
≤0.3 |
≤0.3 |
≤0.3 |
0.15-0.3 |
≤0.3 |
|
LOI |
% |
≤8 |
≤8 |
≤8 |
≤5 |
≤8 |
Bulk Density |
g/ml |
0.68-0.72 |
0.70-0.75 |
0.65-0.75 |
0.70-0.80 |
0.75-0.80 |
Surface Area |
m2/g |
≥300 |
≥300 |
260-300 |
≥300 |
≥300 |
Pore Volume |
ml/g |
0.30-0.45 |
0.30-0.42 |
0.40-0.46 |
0.4 |
0.30-0.50 |
Static Absorption (RH=60%) |
% |
Water Absorption |
Fluorine Absorption |
Water Absorption |
Water Absorption |
Water Absorption |
17-19 |
0.2-0.3 |
50 |
50-70 |
17-19 |
||
Active |
% |
|
|
56-62 |
|
|
Attrition Loss |
% |
≤1.0 |
≤1.0 |
≤1.0 |
≤0.4 |
≤0.8 |
Crushing Strength (mm) |
0.4-1.2mm |
|
≥30 |
|
|
|
1-2mm |
≥40 |
≥40 |
|
|
|
|
2-3mm |
≥70 |
≥70 |
|
|
|
|
3-5mm |
≥150 |
|
≥150 |
≥150 |
≥150 |
|
4-6mm |
≥180 |
|
≥180 |
≥180 |
≥180 |
|
5-7mm |
≥200 |
|
|
|
≥200 |
|
6-8mm |
≥300 |
|
|
|
≥300 |
|
8-10mm |
≥350 |
|
|
|
|
|
10-13mm |
≥350 |
|
|
|
|
|
12-14mm |
≥350 |
|
|
|
|
|
Typical Application |
KA401: is for as adsorbent |
|||||
KA402: is for defluorinating |
||||||
KA403: is for absorption in producing hydrogen peroxide (H2O2) |
||||||
KA404: is for catalyst carrier |
||||||
KA405: is for dehydrating and drying in air separation etc. |
Package shipping
Previous: 13X APG Molecular Sieves
Next: No more